COMPOSITION:
POWDER:
LIQUID:
ADVANTAGES:
1. Dispensing Powder and Liquid
1 . For cementation (Standard Powder/Liquid Ratio: 1.7g / 1.0g)
Dispense one level scoop of Powder using the measuring scoop provided and four drops of Liquid, separately.
2. For lining (Standard Powder/Liquid Ratio: 2.3g / 1.0g)
Dispense one level scoop of Powder using the measuring scoop provided and three drops of Liquid, separately.
2. Mixing
Dispense Powder and Liquid onto a thick glass slab. Divide dispensed powder into 2 equal portions; introduce the first half to the dispensed liquid and mix using a stainless steel spatula. Then, add the remaining half and mix until it becomes homogeneous paste.
Mixing temperature : 23±1ºC?73.4±1.8 ºF? Mixing time : 30 – 40 sec
3. Cementation / Lining
Perform cementation or lining following the conventional method.